Darkroom Variables with Classic Cyanotype – Waiting time from coating to printing.

  • I coated a sheet of paper using a rod and very little emulsion (0,0025 ml/cm2) down to where I drew the pencil lines. I cut the sheet in four strips when dry. 
  • Room temperature was 22 deg C and Relative Humidity 74%. 
  • I waited 20 minutes from coating and printed the first quarter of the coated sheet (Test strip 415c) for 1 minute (a shorter exposure time than my standard so to better see any color variation when comparing it with the other prints). 
  • I covered a part of the coating with an opaque material to have a non exposed area where to check fogging.
  • I waited 40 minutes from coating before printing the second quarter of the sheet as above (Test strip 416c).
  • I waited 60 minutes from coating for the third quarter as above (Test strip 418c).
  • I waited 80 minutes from coating for the fourth quarter as above (Test strip 417c).

P.S. yes I mismatched the strips already numbered when printing so they are not in sequence, but correct.

At the end of the test I could see there was no difference in dMax (color density) in the four prints and the fog under the covered part was pretty similar and almost absent.

In my conclusions there is not much difference if you wait for 20 or 80 minutes to print after coating. 

P.P.S.  I always suggest not to wait too long from coating to printing otherwise fogging may become evident in some circumstances (depending on quantity of emulsion used and R.H. of your place) and your paper white may be less white, or gone. 

I tend to always wait from 45 to 60 min for consistency in my darkroom variables, the base for a perfect digital negative.

This is an external resource for cyanotype printing of the Digital Negative video course. You can read more about it clicking HERE.

Darkroom Variables with Classic Cyanotype – Alkaline buffered (acid free) papers

I used only acid free papers for quite a long time, before I started buying Arches Platine, a pure cotton rag with no alkaline reserve that gives me wonderful results with blue and turquoise shades.

Acid free papers such as watercolor papers often give very dark blues, even darker than Arches Platine and they are much cheaper, but they tend to bleach out when printing in cyanotype unless you adopt some countermeasures.

You have two ways to do so:

  • pre acidify your sheets of paper before using them for printing
  • compensate for the alkaline buffer when developing and washing your print.

I never pre acidify my paper because I don’t want to spend time working twice on a sheet of paper, but it might be the best practice, in fact if you pre acidify you end up printing with a neutral paper and this makes things good and easy.

If you coat your buffered paper the way it comes and print on it when the emulsion has dried, let’s say after one hour or so, you can perfectly compensate for the alkaline buffer when you develop and wash your paper immediately after printing.

In my tests I found that the alkaline buffer of Canson XL Aquarelle (or Watercolor, name depends on what market it is sold) can be perfectly compensated using 0,3 g/l of sulfamic acid put in all the dev. and washing baths, for at least 15 minutes, but 20 minutes are better for a complete wash.

Before Canson, I also used other buffered papers such as Fabriano Accademia and Caballo 109, and I always compensated for their alkaline buffer during wash.

Sulfamic acid has good properties when used with paper because it doesn’t interact badly with the paper itself and has no smelling fumes (unlike chloridric acid that I used when I began printing). But sulfamic acid is not super soluble so you need to warm up some water, up to 60-70 degrees Celsius (140-160 F), and then pour it on your acid crystals inside a capable container, then stir for a few minutes until complete dissolution.

I make a rough 10% solution (not exact in chemical practice) using 90 g of sulfamic acid crystals and 900 ml of water (0,9 liter).

When developing and washing the print that you have made on Canson XL Aquarelle (Watercolor) you need to put 3 ml of the sulfamic acid solution you have previously prepared per each liter of water you put in your trays.

For 20×30 cm (8×12 inches ca.) prints on Canson and classic cyanotype my 3 small trays are configured this way:

  1. 2 liters of water with 3 ml/l (in 10% solution) sulfamic acid, constantly rocking by hand for 1 minute (there is a lot of wash off).
  2. 2 liters of water with 3 ml/l (in 10% solution) sulfamic acid, rocking by hand for 4 minutes.
  3. 2 liters of water with 3 ml/l (in 10% solution) sulfamic acid, rocking (but less) by hand for 15 minutes.

You need to change the water in the first tray for each print (it gets very dirty) and you can use the water inside the second and third tray (with two liters of washing water each) for a maximum of three prints, this is because during washing the acid is slowly neutralized while compensating the alkaline buffer of the paper, so you need to have fresh water and acid to be always effective in washing the print and getting rid of the alkaline buffer.

If you want to use another type of acid, like citric acid (the worst option is chloridric acid), you’ll need to experiment with the quantities I suggested, since each acid has a different pH when diluted in water and so a different compensating ability.

If you want to use white vinegar you need to experiment too, you’ll need way more quantity.

Everything must be tested, defined and then kept consistent in your printing process, that is the base for a perfect digital negative.

This is an external resource for cyanotype printing of the Digital Negative video course. You can read more about it clicking HERE.

Darkroom Variables with Classic Cyanotype – Development and Washing

Washing your cyanotype in the best way is very important in order to have a print that will last beautifully.

If you don’t wash enough, some emulsion will remain inside the paper and it will show up in time as a yellow cast in the highlights. 

If you wash too much, you risk to wash off a bit of the darker areas of your print and so to reduce its overall contrast.

Water temperature, water pH, washing time, speed of agitation (rocking) are all factors that may give you a difference. You want to find your own way to develop and wash and keep it consistent, from the first test prints during the digital negative calibration to your real photo prints, because also from that depends the reliability of your digital negative calibration, and at the end the quality of your print.

I found that for my process with Arches Platine (a process consists of the sum of all the darkroom and printing variables including emulsion type, paper type, relative humidity, type of coating, etc) the best washing time was 20 minutes in total. 

My tap water is alkaline and to compensate it I need to use a little citric acid as follows. This is valid only for me, you need to check the pH of your tap water, for that I suggest you to use the liquid tests for aquariums which are more reliable than the paper strips. Also, I use a certain quantity of citric acid in the first development tray to widen the exposure scale in my prints but I’ll write more on that in a specific post.

For a 30×40 cm (12×16 inches ca.) print on Arches Platine and classic cyanotype my 3 trays are configured this way:

  • first tray: 2 liters of water with 5 ml/l (in 10% solution) citric acid, constantly rocking by hand for 3 minutes, print face up to avoid air bubble formations, with a continuous and rather quick (but not too much) rocking at least in the first minute when developing occurs to prevent staining from bleeding.
  • second tray: 10 liters of water with 0,3 ml/l (in 10% solution) citric acid, I use a small submerged aquarium pump because I get bored, (hence the 10 liters, otherwise 5 liters are enough if my pump can stay beside the print inside my tray) for moving water for 3 minutes, print face down, to clear most of the emulsion.
  • third tray: 5 liters of water with 0,3 ml/l (in 10% solution) citric acid, gently rocking by hand from time to time for the last 14 minutes, print face down.

For smaller prints like 25×25 cm (10×10 inches) I use 2 liters, 5 liters and 5 liters respectively in my 3 trays and if the prints are smaller I reuse the water of the second and third tray for washing more prints. I always change the water in the first tray for each print.

Washing for a total of 15 minutes was also good but the paper white was best at 20 mins, so that’s my washing variable defined for a perfect digital negative.

This is an external resource for cyanotype printing of the Digital Negative video course. You can read more about it clicking HERE.

Negativo Digital para Fotografía Alternativa

For English click here.

Soy feliz de ofrecerte el primer video curso profesional para hacer Negativos Digitales para Fotografía Alternativa. Es en Inglés con subtítulos en Inglés y en Castellano.

Para descubrir el curso haz click AQUÍ.

La preparación de este video curso ha llevado más de un año y medio. Mi experiencia previa, haciendo miles de impresiones utilizando negativos digitales, ha sido indispensable para comprender realmente todos los detalles que ahora puedo explicarte. Antes de tener la idea de hacer este video curso hice muchísimas pruebas para ampliar mi conocimiento sobre la linealización de un negativo digital y dominar todas las variables conectadas en imprimir en mi proceso, así para poder tener resultados bonitos y constantes. Trabajar con John Isner ha sido de gran ayuda.

Empecé en 2016 usando una impresora barata todo-en-uno y una manera basica para preparar mis negativos digitales. Vendía muchas impresiones y en 2017 mejoré mi equipamiento. Compré una cámara de formato completo, una impresora Epson P600, una nueva insoladora UV (hecha a mano) que bajaba mis tiempos de exposición. Compré una Tabla de Pasos Stouffer (step wedge) y preparé una tabla de tiempos sencilla da utilizar para hacer pruebas manuales de tiempos de exposición. Hice a mano un ” UV Dose Meter” para medir la exposición variable del sol. Escogí es sistema Easy Digital Negatives (EDN) de Peter Mrhar para calibrar mis negativos digitales así que podía concentrarme en editar mis fotos sin la necesidad de hacer todas las mediciones técnicas. En el curso utilizaré algunas herramientas modernas de EDN, independientes del editor de fotos que elijas, que son accesibles gratuitamente en la web.

This image has an empty alt attribute; its file name is neg-and-print-centollo.jpg
el negativo calibrato con su color bloqueador óptimo (EDN) y la impresión final en cianotipia clásica sobre Arches Platine



Necesitas saber como calibrar tu negativo digital si imprimes en procesos de fotografía alternativa como la Platinotipia, Cianotipia, Van Dyke Brown, Calitipia, Papel Salado, Crisotipia, Gum bichromate, Argirotipia, Impresión al Carbón, etc.

He abierto este video curso a los miembros de AlternativePhotography.com antes de hacerlo público. Muchos me ayudaron con sus interesantes comentarios. He tenido el honor de recibir reseñas de 5 estrellas por esos expertos profesionales!

This image has an empty alt attribute; its file name is review-1.png

Encontrarás muchas informaciones detalladas, y en cada lección hay un espacio donde poner preguntas a las que yo contestaré. Aunque el valor de este curso es alto he decidido, como es mi politica personal, de ofrecerlo al precio más bajo posible para mi, así que el más amplio público posible pueda inscribirse y disfrutarlo. Tienes acceso garantizado ilimitado de por vida cuando lo compras! Estoy seguro que ya has comprobado otros talleres (workshops) para hacer negativos digitales (dos o tres días prácticos) con precios hasta cienes o miles de dólares.

Para saber más y descubrir el video curso sobre el Negativo Digital haz click AQUÍ. Hay un video de introducción, que puedes ver gratuitamente antes de comprar, que describe conceptos importantes y los pasos del curso.

Está alojado en Thinkific, una plataforma profesional para video cursos que utiliza plataformas de pago con los protocolos más seguros tal como Stripe para las cartas de crédito y PayPal. Espero que te gustará el camino.

Empezamos! Camina conmigo en pasos sencillos.

Te ofrezco un paquete de “Personal Assistance” para ayudarte a crecer como impresor con tus cianotipos o para acelerar tu aprendizaje en la calibración de tu negativo digital.

El precio es de 35 Euros por 1 hora de Personal Assistance que puede ser a través de videollamadas en Zoom o Google Meet, o con correo electrónico, o con WhatsApp. Acepto pagos via PayPal, VISA o transferencia bancaria. Por favor contáctame aquí para hablarlo en detalle y concretar el pago de un paquete de Personal assistance.